Rebar (short for reinforcing bar) is a steel bar cast inside concrete to carry the tension forces that concrete cannot carry on its own. Concrete is strong when it is squeezed but cracks easily when it is pulled, so rebar is placed where a slab, beam, footing or wall will be pulled apart under load.
This guide covers what rebar does, what it is made of, the ASTM grades sold in the US, how to read the marks rolled onto every bar, and the coated and non-steel alternatives. Standards and marking rules were checked on November 15, 2026.
Why Concrete Needs Rebar
Picture a concrete beam spanning between two supports with a load in the middle. The beam sags. The top edge gets shorter (compression) and the bottom edge gets longer (tension). Concrete handles the top just fine. The bottom is the problem: concrete’s tensile strength is only a small fraction of its compressive strength, so the bottom face cracks almost as soon as the beam starts to bend.
Steel bars placed near the bottom face take over once the concrete cracks. The concrete still does the compression work at the top; the steel does the tension work at the bottom. The two materials act together because the concrete grips the bar’s ribs and because steel and concrete expand and contract by similar amounts as temperature changes, so the bond is not torn apart by every hot day.
The same logic decides where bars go in other members. A cantilevered balcony bends the other way, so its main bars sit near the top. A footing spreads a column load into the soil and bends upward between the column and its edges, so its bars run along the bottom. Walls and slabs also get bars to control cracking from shrinkage and temperature, even where bending is small. If the bending idea is new to you, our article on how a cantilever beam carries load walks through it with diagrams.
What Rebar Is Made Of
Standard US rebar is hot-rolled steel. Two ASTM specifications cover nearly all of it:
- ASTM A615 covers deformed and plain carbon-steel bars for concrete reinforcement. This is the ordinary bar on most residential and commercial jobs.
- ASTM A706 covers deformed and plain low-alloy steel bars. Its scope says it limits chemical composition and carbon equivalent “to enhance the weldability of the material,” and it also restricts tensile properties for applications such as seismic frames.
The ASTM A615 scope and the ASTM A706 scope both describe the product as bars “in cut lengths and coils for concrete reinforcement.” Carbon and alloy content are what separate the two: A706 trades a little chemistry freedom for predictable welding and ductility.
Why the bars have ribs
The raised ribs on rebar are called deformations. A smooth bar could slip through hardened concrete like a rod in a tube; the ribs lock the bar into the concrete so load passes from one material to the other. Plain (smooth) bars still exist in both specifications, but they are used for specific purposes such as dowels that are meant to slide, not for main tension reinforcement.
Rebar Grades
The grade number is the minimum yield strength in thousands of psi (ksi). A Grade 60 bar is guaranteed not to start yielding below 60,000 psi. The current scopes list these grades (checked November 15, 2026):
| Grade (inch-pound) | Metric grade | Minimum yield | ASTM A615 (carbon) | ASTM A706 (low-alloy) |
|---|---|---|---|---|
| 40 | 280 | 40,000 psi (280 MPa) | Yes | No |
| 60 | 420 | 60,000 psi (420 MPa) | Yes | Yes |
| 80 | 550 | 80,000 psi (550 MPa) | Yes | Yes |
| 100 | 690 | 100,000 psi (690 MPa) | Yes | Yes |
Grade 60 is the default in most US construction documents. A higher grade does not make concrete members automatically stronger: the engineer sizes the bars, spacing and concrete together, and swapping in a different grade or bar size changes the design. For what “yield” means and why it matters more than ultimate strength, see our guide to the yield strength of steel.
Rebar Sizes in Brief
US bars are called by a number: #3, #4, #5 and so on. For bars #3 through #8, the number is the nominal diameter in eighths of an inch, so a #4 bar is 4/8 = 1/2 in and a #5 is 5/8 in. From #9 up the sizes no longer follow the eighths rule exactly. Diameters, areas and weights per foot for every size, with metric equivalents, are in our rebar size chart.
How to Read the Marks on a Bar
Every deformed bar carries rolled-in marks so it can be identified after delivery. According to the CRSI bar identification guide (checked November 15, 2026), the marks appear in this order:
- Mill mark: a letter or symbol for the producing mill.
- Bar size: the size number.
- Type:
Sfor carbon steel (A615) orWfor low-alloy steel (A706). - Grade: either a number or a system of continuous lines.
| Grade line marking | Grade |
|---|---|
| One line | Grade 60 |
| Two lines | Grade 75 |
| Three lines | Grade 80 or Grade 100 |
| Four lines | Grade 120 |
The W mark matters if anyone plans to weld. The A706 scope limits chemistry and carbon equivalent for weldability and recommends the AWS D1.4 reinforcing-steel welding code. A615 bar has no such limit, so never weld or tack rebar unless the engineer has approved it and a written welding procedure is in place.
Types of Rebar
Bare steel bar (“black bar”) is protected by the alkaline concrete around it. Where chlorides from de-icing salt or sea water can reach the steel, designers often specify a coating or a different material.
| Type | What it is | Where it is used | Watch out for |
|---|---|---|---|
| Black (uncoated) bar | Plain A615 or A706 steel | Most footings, slabs, walls and beams | Relies on concrete cover for corrosion protection |
| Epoxy-coated | Steel bar with a fused epoxy coating, usually green | Bridge decks, parking garages, marine work | Coating damage from handling, cutting or bending must be touched up |
| Galvanized | Steel bar hot-dip coated with zinc | Exposed architectural concrete, coastal work | Cut ends lose the zinc and need repair |
| Stainless steel | Bar made from stainless alloy | Long-life structures in severe chloride exposure | Much higher material cost |
| GFRP | Glass-fiber reinforced polymer bar, not steel | Where corrosion or magnetic interference is a concern | Cannot be bent on site; different design rules |
For how zinc protects steel and why a scratch does not immediately rust, see what galvanized steel is.
Rebar on Site: The Basics That Go Wrong
- Cover: the concrete between the bar and the outside face is part of the design. Too little and the bar rusts and spalls the concrete; too much and the bar sits closer to the middle of the member, where it does less work. Bars are held at the right height on chairs or concrete blocks, not lifted with a rake during the pour.
- Laps: where two bars overlap to continue a run, the lap length is set by the engineer. Short laps are a common inspection failure.
- Bends: bars are bent around a minimum pin diameter. Bending too tightly, or heating a bar to bend it, can crack or weaken it.
- Cleanliness: light surface rust is normal; loose scale, mud or oil weakens the bond.
- Exposed ends: cut bar ends sticking up are an impalement hazard and need caps or covers. Our guide on how to cut rebar covers cutting methods and end protection.
Bar size, grade, spacing, cover and lap lengths for any structural element must come from the drawings or from a licensed structural engineer. Building codes reference ACI 318 for reinforced concrete design, and a local building department will inspect reinforcement before the pour on permitted work.
Frequently Asked Questions
What is rebar made of?
Standard US rebar is hot-rolled carbon steel to ASTM A615 or low-alloy steel to ASTM A706. Coated versions add epoxy or zinc to a steel bar, stainless bar uses a stainless alloy, and GFRP bar is a glass-fiber composite with no steel at all.
What does the “S” or “W” on rebar mean?
It is the steel type. S means carbon-steel bar to ASTM A615; W means low-alloy bar to ASTM A706, which has controlled chemistry for better weldability.
What grade of rebar is most common?
Grade 60 (60,000 psi minimum yield) is the usual specification in US construction. It is marked with the number 60 or a single continuous line along the bar.
Does rebar rust inside concrete?
Concrete’s alkalinity normally protects embedded steel. Rust starts when chlorides or carbonation reach the bar, usually through thin cover or cracks. Once the bar rusts it expands and can crack the concrete off, which is why cover depth and coated bars matter in salty or wet exposures.
Can I use rebar as a beam or post?
Rebar is designed to work inside concrete, not on its own. A bare bar is slender and buckles easily in compression. For a free-standing steel member, look at structural shapes such as steel columns or tube, sized by a licensed structural engineer.
The Short Version
Rebar is ribbed steel bar that gives concrete the tensile strength it lacks. Most US bar is ASTM A615 carbon steel or A706 low-alloy steel, Grade 60 is the common grade, and the marks on each bar tell you the mill, size, type and grade. Where and how much rebar goes into a member is an engineering decision, not a rule of thumb.
Reference information only, not engineering advice. Disclaimer.