Oil canning is the visible waviness that shows up in the flat areas of metal roof and wall panels. It is caused by uneven stresses locked into the sheet, and in most cases it is a cosmetic issue rather than a structural or leak problem.
This guide explains what oil canning is, where the stresses come from (from the steel mill to the installer’s screw gun), which panels are most prone to it and what reduces it. The main source is the Metal Construction Association’s technical bulletin on the subject, checked on November 17, 2026.
What Oil Canning Is
The MCA technical bulletin “Oil Canning in Metal Roof and Metal Wall Systems” defines it as visible waviness in the flat areas of metal panels. The technical name is elastic buckling, and the bulletin treats waviness, stress wrinkling and oil canning as the same thing. It can happen in steel, aluminum, zinc or copper panels.
The name comes from the old metal oil can: press the thin side and it pops in, release it and it pops back. A panel with oil canning has a flat area that has buckled slightly out of plane, so light reflects off it unevenly. The waves are often only noticeable at certain times of day, from certain angles or on certain colors, and the bulletin notes that if oil canning is present, it is usually apparent at the time of construction.
What Causes Oil Canning
Oil canning is caused by differential stresses within the metal. When a thin, wide flat area tries to relieve those stresses, it buckles out of plane. The MCA bulletin groups the sources of stress into four stages.
1. Coil production at the mill
Roof and wall panels start as thin sheet rolled under pressure and wound into coils. Rolling is never perfectly even. The bulletin names three common conditions: full center (the middle of the strip is longer than the edges), wavy edge (the edges are longer than the middle) and camber (a side edge that curves away from a straight line). All light-gauge coil has some of each, and the effect grows as tensile strength rises. Our article on hot rolled vs cold rolled steel explains how sheet is rolled down to these thicknesses.
2. Slitting and roll forming
A wide master coil is usually slit into narrower coils, which releases and redistributes the stresses already in the steel. Roll forming then bends the edges into ribs or seams while the middle stays flat. Architectural profiles need much more forming at the edges than in the center, which tends to trap uneven stress in the flat pan. Corrugated and ribbed profiles are usually formed from the center outward, which pushes the stress toward the edges. Together with their narrow flat sections, that is one reason ribbed and corrugated metal panels are less prone to it.
3. The structure underneath
Panels forced to conform to supports that are not in one plane pick up extra stress, even when the framing is within normal tolerances. The bulletin lists three cases: misaligned supports or perimeter framing; movement of the primary structure from deflection, racking, drift or settlement; and intentional camber in rafters, trusses or joists that leaves a crowned surface. On a metal building, the line of the purlins is part of what the finished roof looks like.
4. Installation, heat and handling
- Over-engaged roof panels. Panels pulled tighter than their design coverage width lose the flex in the ribs and seams that absorbs sideways movement.
- Overdriven fasteners. Screws driven too hard dimple the sheet and can show as waves along the fastener lines.
- Restrained thermal movement. Panels grow and shrink along their length every day. The bulletin notes panel surfaces can run more than 100 degrees above air temperature. Flashings or “dual pinning” that lock both ends stop that movement and produce waves that can come and go during the day.
- Storage and handling. Carrying panels flat, twisting them or lifting by one corner can put a permanent wave into a previously flat panel.
Which Panels Are Most Prone to It
| Factor | More prone to visible oil canning | Less prone |
|---|---|---|
| Flat width | Wide flat pans | Narrow pans, ribbed or corrugated profiles |
| Thickness | Thinner sheet (higher gauge number) | Thicker sheet (lower gauge number) |
| Coil flatness | Standard coil | Tension-leveled coil |
| Finish | High-gloss | Low-gloss or embossed |
| Color | Dark colors | Light colors |
| Attachment | Fixed at both ends, overdriven screws | Clips that allow thermal movement |
Steel sheet thickness is usually ordered by gauge, and a lower gauge number is thicker. For the actual thickness behind each number, see our steel gauge thickness chart.
How to Reduce Oil Canning
No manufacturer or installer can promise a panel with zero oil canning. The MCA bulletin is direct about that. What you can do is lower the odds and make any waviness less visible.
- Order tension-leveled material. Tension (stretch) leveling pulls the coil past its yield point so it cannot creep back to its uneven shape. The bulletin recommends it be done after slitting. Our article on the yield strength of steel explains what stretching past yield means.
- Go thicker. In general, the thicker the metal, the less likely the panel is to oil can.
- Choose a profile with stiffening ribs. Striations or pencil ribs break up the flat area. They may add faint shadow lines of their own.
- Narrow the pan. The waves get more pronounced as the flat width increases.
- Pick a low-gloss, embossed or lighter finish. Less reflective surfaces hide the waves, and dark colors show them most.
- Specify flat supports. The bulletin notes normal trade tolerances for the substrate may not be tight enough. Tighter alignment specs for the deck or purlins focus attention on this.
- Use backer rod where the system allows it. Some designers specify foam backer rod under the pan on a solid deck so the pan “pillows” evenly.
- Install to the manufacturer’s instructions. Correct coverage width, correct screw torque, clips and flashings that let panels move, and careful handling.
Is Oil Canning a Defect?
Usually not. The concluding remarks of the bulletin (the full PDF, also hosted by panel maker McElroy Metal as the MCA tech sheet) say oil canning is generally an aesthetic issue, structural integrity is typically not affected, and in the absence of specific contract requirements it should not be the sole grounds for panel rejection. Some designers even accept it as a natural look of the material.
Waviness is different from damage. Dents from hail or foot traffic, panels pulling off their clips, open seams or leaks are not oil canning. If a roof shows sudden new waviness, especially after a storm, heavy snow or work on the structure, have it inspected. Movement of the primary structure is one of the listed causes, and a licensed structural engineer should check framing that may be deflecting or settling.
Frequently Asked Questions
Can oil canning be fixed after installation?
Sometimes. Waves along overdriven fasteners or from flashings that pin the panel may improve once the cause is corrected. Waves built into the coil or forced by uneven supports are harder to fix. The MCA notes that if the cause is the support system, even replacing the panels may not help unless the root cause is addressed.
Does oil canning cause leaks?
Oil canning itself is waviness in the flat of the panel, away from the seams, and the MCA describes it as generally aesthetic. A leak points to a seam, fastener, flashing or penetration problem, which needs its own inspection.
Why does my metal roof look wavy only in the morning?
Two reasons. Low sun angles make small waves much more visible, and thermal waves can appear and disappear during the day as the panels heat and cool. Neither means the panels are changing shape for good.
Does Galvalume or galvanized steel oil can more?
The coating is not the cause. Oil canning comes from stresses in the base sheet, its width and thickness, and the installation. Gloss and color do change how visible it is, so a shiny bare Galvalume panel can show the same waves more clearly than a low-gloss painted one.
The Short Version
Oil canning is waviness in the flat areas of metal panels caused by uneven stresses from the mill, the roll former, the supporting structure or the installation. It is mostly cosmetic. Thicker, tension-leveled sheet, narrower or ribbed pans, low-gloss finishes, flat supports and careful installation all reduce it, but none can guarantee it will not appear.
Reference information only, not engineering advice. Disclaimer.